  • Gap between two coils – 120 mm & distance between coil & refractory wall – 95mm.
  • Multiple weld defects in the existing joints leading to leak in Nitrogen pressure test
  • Technical discussion with client and development of repair procedure
  • Successful implementation of the developed procedure to customer satisfaction